Czasopisma
Czasopisma
Czasopisma
ATEST - OCHRONA PRACY
ATEST - OCHRONA PRACY
AURA
AURA
AUTO MOTO SERWIS
AUTO MOTO SERWIS
CHEMIK
CHEMIK
CHŁODNICTWO
CHŁODNICTWO
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
DOZÓR TECHNICZNY
DOZÓR TECHNICZNY
ELEKTROINSTALATOR
ELEKTROINSTALATOR
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
Czasopisma
Czasopisma
Czasopisma
GAZETA CUKROWNICZA
GAZETA CUKROWNICZA
GAZ, WODA I TECHNIKA SANITARNA
GAZ, WODA I TECHNIKA SANITARNA
GOSPODARKA MIĘSNA
GOSPODARKA MIĘSNA
GOSPODARKA WODNA
GOSPODARKA WODNA
HUTNIK - WIADOMOŚCI HUTNICZE
HUTNIK - WIADOMOŚCI HUTNICZE
INŻYNIERIA MATERIAŁOWA
INŻYNIERIA MATERIAŁOWA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MATERIAŁY BUDOWLANE
MATERIAŁY BUDOWLANE
OCHRONA PRZED KOROZJĄ
OCHRONA PRZED KOROZJĄ
ODZIEŻ
ODZIEŻ
Czasopisma
Czasopisma
Czasopisma
OPAKOWANIE
OPAKOWANIE
PACKAGING REVIEW
PACKAGING REVIEW
POLISH TECHNICAL REVIEW
POLISH TECHNICAL REVIEW
PROBLEMY JAKOŚCI
PROBLEMY JAKOŚCI
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
Czasopisma
Czasopisma
Czasopisma
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ SPOŻYWCZY
PRZEMYSŁ SPOŻYWCZY
RUDY I METALE NIEŻELAZNE
RUDY I METALE NIEŻELAZNE
SZKŁO I CERAMIKA
SZKŁO I CERAMIKA
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
WIADOMOŚCI ELEKTROTECHNICZNE
WIADOMOŚCI ELEKTROTECHNICZNE
WOKÓŁ PŁYTEK CERAMICZNYCH
WOKÓŁ PŁYTEK CERAMICZNYCH
Menu
Menu
Menu
Prenumerata
Prenumerata
Publikacje
Publikacje
Drukarnia
Drukarnia
Kolportaż
Kolportaż
Reklama
Reklama
O nas
O nas
ui-button
Twój Koszyk
Twój koszyk jest pusty.
Niezalogowany
Niezalogowany
Zaloguj się
Zarejestruj się
Reset hasła
Czasopismo
|
INŻYNIERIA MATERIAŁOWA
|
Rocznik 2015 - zeszyt 6
Analiza mikrostruktury stali podeutektoidalnej Co-Mo po ciągłym chłodzeniu z zakresu austenitu
10.15199/28.2015.6.13
Edyta Rożniata
Rafał Dziurka
Kamil Górecki
nr katalogowy: 95616
10.15199/28.2015.6.13
Analysis of the microstructure of the hypoeutectoid Co-Mo steel after continuous cooling from austenite range Present work corresponds to the research on the kinetics of phase transformation of undercooled austenite and analysis of the microstructure of 37CoMo4-3 hypoeutectoid steel, imitating by its chemical composition toughening steels. The kinetics of phase transformation of undercooled austenite of investigated alloy was presented on CCT diagram (continuous cooling transformation). The paper presents metallographic examinations, as well as hardness measurements. Metallographic observations were carried out using a Carl Zeiss Axiovert 200 MAT light microscope. Polished sections were etched with a 3% nital (3% HNO3 solution in C2H5OH). Dilatometric tests were performed using L78 R.I.T.A dilatometer of LINSEIS. Using dilatometer, the changes of elongation of the samples with dimensions Ø3×10 mm as a function of temperature were registered. Obtained heating curves were used for precise determination of the critical temperatures (critical points) for the examined steels. The differentiation of obtained cooling curves allowed to precisely define the temperature of the beginning and the end of particular phase transitions and thus to draw CCT diagrams. Key words: hypoeutectoid steel, microstructure, kinetics of phase transformation, CCT diagram, heat treatment. W pracy przedstawiono analizę kinetyki przemian fazowych przechłodzonego austenitu stali podeutektoidalnej 37CoMo4-3. Zastosowano badania metalograficzne oraz dylatometryczne, a także pomiary twardości. Badania metalograficzne wykonano na mikroskopie świetlnym Axiovert 200 MAT firmy Carl Zeiss. Zgłady trawiono 3% nitalem w celu ujawnienia poszczególnych składników mikrostrukturalnych badanej stali. Pomiary twardości wykonano aparatem Vickersa typu HPO 250, stosując siłę obciążająca 30 kG. Badania dylatometryczne wykonano za pomocą dylatometru L78 R.I.T.A. firmy LINSEIS. Rejestrowano[...]
Treść płatna
Jeśli masz wykupiony/przyznany dostęp -
zaloguj się
.
Skorzystaj z naszych propozycji zakupu!
Publikacja
e-Publikacja (format pdf) - nr 95616 "Analiza mikrostruktury st..."
licencja: Osobista
Produkt cyfrowy
10.00 zł
Do koszyka
Zeszyt
INŻYNIERIA MATERIAŁOWA - e-zeszyt (pdf) 2015-6
licencja: Osobista
Produkt cyfrowy
65.00 zł
Do koszyka
Prenumerata
INŻYNIERIA MATERIAŁOWA - prenumerata cyfrowa
licencja: Osobista
Produkt cyfrowy
Nowość
402.00 zł
Do koszyka
INŻYNIERIA MATERIAŁOWA - papierowa prenumerata roczna + wysyłka
licencja: Osobista
Szczegóły pakietu
Nazwa
INŻYNIERIA MATERIAŁOWA - papierowa prenumerata roczna
492.00 zł brutto
455.56 zł netto
36.44 zł VAT
(stawka VAT 8%)
INŻYNIERIA MATERIAŁOWA - pakowanie i wysyłka
21.00 zł brutto
17.07 zł netto
3.93 zł VAT
(stawka VAT 23%)
513.00 zł
Do koszyka
INŻYNIERIA MATERIAŁOWA - PAKIET prenumerata PLUS
licencja: Osobista
Szczegóły pakietu
Nazwa
INŻYNIERIA MATERIAŁOWA - PAKIET prenumerata PLUS
600.00 zł brutto
555.56 zł netto
44.44 zł VAT
(stawka VAT 8%)
600.00 zł
Do koszyka
Zeszyt
2015-6
Czasopisma
ATEST - OCHRONA PRACY
AURA
AUTO MOTO SERWIS
CHEMIK
CHŁODNICTWO
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
DOZÓR TECHNICZNY
ELEKTROINSTALATOR
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
GAZETA CUKROWNICZA
GAZ, WODA I TECHNIKA SANITARNA
GOSPODARKA MIĘSNA
GOSPODARKA WODNA
HUTNIK - WIADOMOŚCI HUTNICZE
INŻYNIERIA MATERIAŁOWA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MATERIAŁY BUDOWLANE
OCHRONA PRZED KOROZJĄ
ODZIEŻ
OPAKOWANIE
PACKAGING REVIEW
POLISH TECHNICAL REVIEW
PROBLEMY JAKOŚCI
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ SPOŻYWCZY
RUDY I METALE NIEŻELAZNE
SZKŁO I CERAMIKA
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
WIADOMOŚCI ELEKTROTECHNICZNE
WOKÓŁ PŁYTEK CERAMICZNYCH