Czasopisma
Czasopisma
Czasopisma
ATEST - OCHRONA PRACY
ATEST - OCHRONA PRACY
AURA
AURA
AUTO MOTO SERWIS
AUTO MOTO SERWIS
CHEMIK
CHEMIK
CHŁODNICTWO
CHŁODNICTWO
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
DOZÓR TECHNICZNY
DOZÓR TECHNICZNY
ELEKTROINSTALATOR
ELEKTROINSTALATOR
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
Czasopisma
Czasopisma
Czasopisma
GAZETA CUKROWNICZA
GAZETA CUKROWNICZA
GAZ, WODA I TECHNIKA SANITARNA
GAZ, WODA I TECHNIKA SANITARNA
GOSPODARKA MIĘSNA
GOSPODARKA MIĘSNA
GOSPODARKA WODNA
GOSPODARKA WODNA
HUTNIK - WIADOMOŚCI HUTNICZE
HUTNIK - WIADOMOŚCI HUTNICZE
INŻYNIERIA MATERIAŁOWA
INŻYNIERIA MATERIAŁOWA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MATERIAŁY BUDOWLANE
MATERIAŁY BUDOWLANE
OCHRONA PRZED KOROZJĄ
OCHRONA PRZED KOROZJĄ
ODZIEŻ
ODZIEŻ
Czasopisma
Czasopisma
Czasopisma
OPAKOWANIE
OPAKOWANIE
PACKAGING REVIEW
PACKAGING REVIEW
POLISH TECHNICAL REVIEW
POLISH TECHNICAL REVIEW
PROBLEMY JAKOŚCI
PROBLEMY JAKOŚCI
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
Czasopisma
Czasopisma
Czasopisma
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ SPOŻYWCZY
PRZEMYSŁ SPOŻYWCZY
RUDY I METALE NIEŻELAZNE
RUDY I METALE NIEŻELAZNE
SZKŁO I CERAMIKA
SZKŁO I CERAMIKA
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
WIADOMOŚCI ELEKTROTECHNICZNE
WIADOMOŚCI ELEKTROTECHNICZNE
WOKÓŁ PŁYTEK CERAMICZNYCH
WOKÓŁ PŁYTEK CERAMICZNYCH
Menu
Menu
Menu
Prenumerata
Prenumerata
Publikacje
Publikacje
Drukarnia
Drukarnia
Kolportaż
Kolportaż
Reklama
Reklama
O nas
O nas
ui-button
Twój Koszyk
Twój koszyk jest pusty.
Niezalogowany
Niezalogowany
Zaloguj się
Zarejestruj się
Reset hasła
Czasopismo
|
HUTNIK - WIADOMOŚCI HUTNICZE
|
Rocznik 2014 - zeszyt 8
Porównanie właściwości mechanicznych i mikrostruktury stali wyskomanganowych z efektem TWIP odkształcanych plastycznie na gorąco
Magdalena JABŁOŃSKA
nr katalogowy: 86590
W artykule zaprezentowano porównanie wyników badań właściwości i mikrostruktury dla dwóch austenitycznych stali wysokomangano- wych, poddanych próbie ściskania na gorąco. Przeprowadzono analizę wpływu parametrów odkształcania plastycznego, takich jak: tempera- tura i prędkość odkształcenia na maksymalne naprężenie uplastyczniające i mikrostrukturę badanych stali. Wykazano zależność maksymal- nego naprężenia uplastyczniającego od prędkości i temperatury odkształcania. W mikrostrukturze obu badanych stali obserwowano efekty charakterystyczne dla procesów dynamicznej odbudowy w trakcie odkształcania na gorąco In the article comparing findings of the property and microstructures were presented for two austenitic high-manganese steels, subjected to the hot compression test. Analysis of the influence of parameters of plastic deformation such steels as the temperature and the strain rate, to properties i.e. the maximum stress and the microstructure examined was conducted. A dependence of the maximum stress on the strain rate and temperatures of deformation were demonstrated. In the microstructure of both examined steels effects characteristic of processes of the dynamic recrystallization are being observed in the course of deformation process. Słowa kluczowe: wysokomanganowa austenityczna stal z efektem TWIP, próba ściskania, właściwości mechaniczne Key words: high manganese austenitic steel with TWIP effect, hot compression test, mechanical properties.Wprowadzenie. Nowoczesny przemysł motory- zacyjny stale dąży do zmniejszenia masy pojazdów nie obniżając przy tym parametrów bezpieczeństwa. Obecnie w odniesieniu do stali dl[...]
Treść płatna
Jeśli masz wykupiony/przyznany dostęp -
zaloguj się
.
Skorzystaj z naszych propozycji zakupu!
Publikacja
e-Publikacja (format pdf) - nr 86590 "Porównanie właściwości me..."
licencja: Osobista
Produkt cyfrowy
10.00 zł
Do koszyka
Zeszyt
HUTNIK - WIADOMOŚCI HUTNICZE - e-zeszyt (pdf) 2014-8
licencja: Osobista
Produkt cyfrowy
32.00 zł
Do koszyka
Prenumerata
HUTNIK - WIADOMOŚCI HUTNICZE - prenumerata cyfrowa
licencja: Osobista
Produkt cyfrowy
Nowość
400.00 zł
Do koszyka
HUTNIK - WIADOMOŚCI HUTNICZE - papierowa prenumerata roczna + wysyłka
licencja: Osobista
Szczegóły pakietu
Nazwa
HUTNIK - WIADOMOŚCI HUTNICZE - papierowa prenumerata roczna
540.00 zł brutto
500.00 zł netto
40.00 zł VAT
(stawka VAT 8%)
HUTNIK - WIADOMOŚCI HUTNICZE - pakowanie i wysyłka
14.00 zł brutto
11.38 zł netto
2.62 zł VAT
(stawka VAT 23%)
554.00 zł
Do koszyka
HUTNIK - WIADOMOŚCI HUTNICZE - PAKIET prenumerata PLUS
licencja: Osobista
Szczegóły pakietu
Nazwa
HUTNIK - WIADOMOŚCI HUTNICZE - PAKIET prenumerata PLUS
600.00 zł brutto
555.56 zł netto
44.44 zł VAT
(stawka VAT 8%)
600.00 zł
Do koszyka
Zeszyt
2014-8
Czasopisma
ATEST - OCHRONA PRACY
AURA
AUTO MOTO SERWIS
CHEMIK
CHŁODNICTWO
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
DOZÓR TECHNICZNY
ELEKTROINSTALATOR
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
GAZETA CUKROWNICZA
GAZ, WODA I TECHNIKA SANITARNA
GOSPODARKA MIĘSNA
GOSPODARKA WODNA
HUTNIK - WIADOMOŚCI HUTNICZE
INŻYNIERIA MATERIAŁOWA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MATERIAŁY BUDOWLANE
OCHRONA PRZED KOROZJĄ
ODZIEŻ
OPAKOWANIE
PACKAGING REVIEW
POLISH TECHNICAL REVIEW
PROBLEMY JAKOŚCI
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ SPOŻYWCZY
RUDY I METALE NIEŻELAZNE
SZKŁO I CERAMIKA
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
WIADOMOŚCI ELEKTROTECHNICZNE
WOKÓŁ PŁYTEK CERAMICZNYCH